Nanoindentation

What is nanoindentation used for?

Nanoindentation is a technique for determining:

Hardness and Young's Modulus: At very small scales (nano to micro).

Creep and Relaxation: Measuring time-dependent deformation under load.

Fracture Toughness: When using indentation fracture techniques.